Designed for welding 1.25% chromium, 0.50% molybdenum steel
Easy slag removal
Premium arc performance
Square coating burn-off
Easy strike, re-strike and slag removal
Capable of exceeding AWS minimum requirement of 550 MPa (80 ksi) tensile strength after 8 hours of stress-relieving at 690°C (1275°F)
Meets AWS minimum requirement of 550 MPa (80 ksi) tensile and 470 MPa (68 Ksi ) yield strength after 48 hours of stress-relieving at 590-620°C (1100-1150°F) as typical in nuclear applications
Each rod is marked with AWS classification and LOT number